Indoor paste in powder (thick coat)

Paste indicated to indoor places to cover surfaces of plaster or cement.
Useful life (S/ITE C1/51-L) 1,5 – 2 Hours
Fire resistante A1- Non combustible
Particle size 300 microns – Medium
pH (S/ITE CI/18-L) 6,5 – 7,5
Shore C Hardness (S/ITE CI/22-L) 81
Storage 12 Months
Tool cleaning With water
Kg of powder used per m2 1 mm thickness 1,16 – 1,19
Kg of paste used per m2 1 mm thickness 1,64 – 1,73
Adhérence (S/Anexxe 2 NF P 74202-1 DTU 59.2)
To acrylic paint Greater than 0,8 MPa
To cement Greater than 0,8 Mpa
Density (S/ITE CI/53-L) Powder 0,92 Gr/Lt
Density (S/ITE CI/53-L) Paste 1,70 Gr/Lt
Drying time in depth (S/ITE CI/52L)
Concrete (Average thickness – 2mm coat) More than 8 hours
Paint (Average thickness – 2mm coat) More than 8 hours
Cement ( Average thickness – 2mm coat) 5-6 hours
Packaging 15 Kg sacks
Conservation Keep away from extreme temperatures

Knead with water at a rate of 43 to 45 percent. For each sack of 15 kg., 6,45 to 6,75 liters of water must be used for his kneading.
The knead must be manually or mechanically using an electric beater. Let the dough a few minutes, then apply. To cover with that block with cavities, a medium-sized spatula, which allows you to press firmly towards the inside of the bowl is recommended. If it is possible, to ensure that the width of the spatula is slightly greater than the size of the cavity.
The smoothing operation always vertically from top to bottom with blade, hardware and remove excess, ensuring smooth and hide all defects on surfaces. Joints are on the contrary, top to bottom. When dry, sanding and then plaster hand will be horizontally from right to left, left to right joints.